Brighton Lock Gate 72” valve Refurbishment
The Brief:
The gate system had developed multiple faults which prevented the seals from operating correctly. Misalignment within the assembly meant the bars were not sealing properly, leading to continued leakage.
During inspection, it became clear that several previous repair methods and component choices were not suitable for the environment or loading conditions. Parts had worn prematurely, hydraulic components had failed and several fabricated sections lacked the strength required for long-term service.
The objective was to fully refurbish and improve the system, as opposed to simply repeating the previous repair approach.
“The objective was to fully refurbish and improve the system, as opposed to simply repeating the previous repair approach.”
The Solution:
Our team carefully removed the lock gate components and carried out a full assessment before beginning the refurb.
The hydraulic seals had completely failed, so new mounting holes were created between the original positions using a right-angle drill due to limited access around the casting.
Because the original bars sat too close to the casting, standard circular components would not fit correctly. We therefore machined bespoke oval-shaped stainless steel discs to achieve the correct clearance while maintaining sealing performance.
A new gland follower was manufactured and fitted, while the valve assembly was rethreaded using a bronze sacrificial thread to improve future serviceability and reduce wear on the parent material.
To correct the alignment of the steel rails, bespoke steel discs were manufactured and fitted to bring the rails back into parallel alignment rather than the bent arrangement previously installed. This allowed the bars to seal correctly against the mating surfaces.
Areas previously repaired using standard filler material were stripped back and rebuilt using ceramic filler, providing a far more suitable long-term repair solution for the operating conditions.
Several thin straps fitted during the previous installation had also failed due to insufficient thickness. We redesigned and remanufactured these components using 10mm stainless steel to provide the required strength and reliability.